December 16, 2020

Hardness below 90A, 3-4 hours at 80℃-90℃

Hardness below 95A, 3-4 hours at 90℃-100℃

When drying, low hardness specification should avoid high temperature and long time for high temperature will cause stick agglomeration and long time drying will make it yellowish


Injection molding temperature reference (Unit ℃ )

Model/Specification
C1 Feed Section
C2 Compression Section
C3 Metering Section
Nozzle
85A 175 180 185 190
95A 180 185 190 195
64D 190 195 200 205
72D 195 205 210 215

Extrusion molding temperature reference (Unit ℃ )

Model/Specification
C1 Feed Section
C2 Compression Section
C3 Metering Section
Nozzle
75A 170 180 180 190
85A 180 185 190 195
95A 185 190 195 200

Characteristic Comparison

Model/Specification
S100 E300 B400 S600 B700
Transparency Good Excellent Excellent
Fair Excellent
Hydrolytic Stability Fair Excellent Excellent
Fair Good
Heat Resistance Good
Fair Excellent
Good Good
Oil Resistance Good
Fair Excellent Good Good
Low Temperature Resistance Good
Excellent
Excellent Excellent
Good
Moldability Good
Fair Good Excellent
Fair
Abrasion Resistance Good
Fair Good Excellent
Good